Waterworks Iron Ore Concentrator (2)

The ore hardness is 12~14, and the rock hardness is 8~10. The ore density is 3.1~3.2t/m 3 and the rock density is 2.7 t/m 3 . The looseness coefficient of ore and rock is 1.5. The ore humidity is generally 0.1 to 0.2% and the maximum is 0.38%.
(2) Process flow: The crushing and screening process of the plant is shown in the following figure. 1. The process of mineral processing is shown in Figure 2 below. The data in the figure is taken from the results of the new three series process in September 1980.



(3) Major technical improvements since the plant was put into production:
1) The operating speed of the heavy-duty plate feeder is increased from 0.05m/s to 0.058m/s, and the ore supply is increased from 1200t/h to 1300t/h, meeting the expansion requirements.
2) Change the rolling wall of the fine crusher to the medium crusher to reduce the product size of the crusher. The fine crusher discharge port is changed from 15mm to 10mm, and the fine crushing cycle load is reduced from 116% to 100%. Below 12mm, the ball mill processing capacity is increased by 0.94t / (unit.h), and the ball mill electromechanical consumption is reduced by 0.22kw.h / t according to the original ore.
3) Improve equipment maintenance work. In 1984, the ball mill operation rate reached 94%.

Wire Cutting Machines

Wire Cutting Machines

JA Series is the upgrade of JC Series, it improved the traditional taper maching accuracy, increased 90° rotating operation panel, with automatic wire feeding structure, make the operation more convenient. The equipment is mostly used in European and American enterprises, military industry, large state-owned enterprises, group companies.

Wire Cutting Machines,Wire Edm Machines,Wire Erosion Machines,Edm Wire Cutting Machines

Ningbo Yien Machinery Co., Ltd , https://www.yiencnc.com